A steady-state thermoreflectance method
to measure thermal conductivity

Research summary · The 2019 paper that introduced SSTR, the steady-state technique behind FASTR

The problem

Engineers measuring thermal conductivity have had to choose between two imperfect options. Steady-state methods measure directly via Fourier’s law but need bulk samples, large heater and sensor areas, vacuum to limit losses, physical contact, and hours to reach steady state. Transient methods such as TDTR, FDTR and 3ω are fast and local but need phase separation and prior knowledge of heat capacity. This paper set out to combine the strengths of both.

The method

Steady-state thermoreflectance (SSTR) heats the sample with a modulated continuous-wave pump laser, and a low-power probe laser reads the surface temperature rise through an 80 nm aluminum transducer film. As pump power increases, the change in probe reflectance tracks the change in heat flux, and Fourier’s law then gives thermal conductivity from the slope. A sapphire wafer sets the calibration.

What the research showed

The team validated SSTR on materials from glass to diamond:

MaterialSSTR (W/m*K)Literature (W/m*K)
Amorphous SiO₂1.13 ± 0.081.3
Z-cut quartz8.63 ± 0.368.6
Sapphire (Al₂O₃)35.0 ± 1.434
Silicon133 ± 6133
4H-SiC310 ± 23364
Diamond1760 ± 3901900

Values are from the paper’s PWA measurements. The measurable range spans about 1 to more than 2000 W/m·K.

Why it matters for your samples

From paper to platform

SSTR is now one of the two measurement modes in FASTR, which pairs it with FDTR. The 2019 setup took seconds to minutes per scan. FASTR’s SSTR mode runs a test cycle in under 1 second.

Jeffrey L. Braun, David H. Olson, John T. Gaskins, and Patrick E. Hopkins, “A steady-state thermoreflectance method to measure thermal conductivity,” Review of Scientific Instruments 90, 024905 (2019). DOI: 10.1063/1.5056182.